Power Diffraction:
Calcit : Ca(CO3)trigonal
Mineralogy: Carbonates calcit more than 99 pct pinel group as magneti Iron Oxide and hydroxides less than 1 pct
Physical properties:
Wet compresive strenhgt: W.C.S. = 802 Kgr.cm-2
Dry Compressive strenhghti: D.C.S. = 932 Kg. cm-2
Elasthchty modulus: E.M. = 5.86 * 10-5 Kg. cm-2
Softening Point: S.P. = 0.81 factor
Hafdhtnin MOH's scale: 3 MOH's
Waterproption coeffiction: 0.6 %
Loss by portshing & cuting: 12.80 %
Expantion & Contraction coefficient:
AT 200 ˚C – 0.19 % AT 40 ˚C – 0.02 %
CaCO3 grade 99.8% in mesh 200 to 1500 in packing Jumbobags